Polymer Property : Melt Index of Compound = 41 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 41 g/10 min

@Load 10.0 kg,
Temperature 280 °C
41 g/10 min

@Load 22.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East)
Melt Index of Compound 41 g/10 min

@Load 2.16 kg,
Temperature 265 °C
41 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 7062HP PBT
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Melt Index of Compound 41 g/10 min

@Load 5.00 kg,
Temperature 300 °C
41 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS
NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory..
Melt Index of Compound 41 g/10 min

@Load 5.00 kg,
Temperature 300 °C
41 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Asia Pacific)
NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory..
Melt Index of Compound 41 g/10 min

@Load 5.00 kg,
Temperature 300 °C
41 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East)
NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory..
Melt Index of Compound 41 g/10 min

@Load 2.16 kg,
Temperature 265 °C
41 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Melt Index of Compound 41 g/10 min

@Load 2.16 kg,
Temperature 265 °C
41 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Melt Index of Compound 41 g/10 min

@Load 5.00 kg,
Temperature 300 °C
41 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Asia Pacific)
EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor..
Melt Index of Compound 41 g/10 min

@Load 5.00 kg,
Temperature 300 °C
41 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Europe-Africa-Middle East)
EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor..
Melt Index of Compound 41 g/10 min

@Load 2.16 kg,
Temperature 280 °C
41 g/10 min

@Load 4.76 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL FP3060 PPE+PS (Europe-Africa-Middle East)
Noryl* FP3060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Melt Index of Compound 41 g/10 min

@Load 2.16 kg,
Temperature 280 °C
41 g/10 min

@Load 4.76 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Melt Index of Compound 41 g/10 min

@Load 2.16 kg,
Temperature 280 °C
41 g/10 min

@Load 4.76 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Melt Index of Compound 41 g/10 min

@Load 2.16 kg,
Temperature 280 °C
41 g/10 min

@Load 4.76 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL PX2060 PPE+PS
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..