Physical Properties Metric English Comments
Melt Index of Compound 14 g/10 min

@Load 2.16 kg,
Temperature 260 °C
14 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS
Color package may affect performance. PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance.
Melt Index of Compound 14 g/10 min

@Load 2.16 kg,
Temperature 260 °C
14 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific)
PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance.
Melt Index of Compound 14 g/10 min

@Load 2.16 kg,
Temperature 260 °C
14 g/10 min

@Load 4.76 lb,
Temperature 500 °F
Honeywell Aegis™ CSD High Barrier Nylon  (discontinued **)
Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET. Information provided by Honeyw..
Melt Index of Compound 14 g/10 min

@Load 2.16 kg,
Temperature 250 °C
14 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East)
VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils.
Melt Index of Compound 14 g/10 min

@Load 2.16 kg,
Temperature 250 °C
14 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
Melt Index of Compound 14 g/10 min

@Load 2.16 kg,
Temperature 300 °C
14 g/10 min

@Load 4.76 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics LNP THERMOCOMP D451 PC (Asia Pacific)
LNP* Thermocomp* D451 (or EXTC8141) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good duc..
Melt Index of Compound 14 g/10 min

@Load 2.16 kg,
Temperature 265 °C
14 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East)
VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles.