Physical Properties Metric English Comments
Carbon Dioxide Transmission 150 cc-mm/m²-24hr-atm
381 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® FG 34 NL nat 6023 PA6
Product description: Grilon FG 34 NL natural 6023 is a modified, medium viscosity polyamide 6. Grilon FG 34 NL natural 6023 exhibits following improvements compared to a PA 6: Better gas barrier pro..
Carbon Dioxide Transmission 150 cc-mm/m²-24hr-atm
381 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® FG 40 NL nat 6025 PA6
Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:Better..