Material Notes:
Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:Better gas barrier properties at elevated humidity and after pasteurization and sterilizationBetter optical and UV- barrier propertiesBetter aroma barrier and flavor protectionBetter thermoforming and orientation properties Application examples: Grilon FG 40 natural 6025 is suitable for production of mono and coextruded cast and blown films Grilon FG 40 natural 6025 is used for the manufacture of oriented films, sausage casings and deep-drawn films. It is also suitable for packaging such as meat cheese and fish (pouches, shells, covers) at elevated humidity levels.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Water Vapor Transmission 10.0 g/m²/day
0.644 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 25.0 cc/m²/day
1.61 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
30.0 cc/m²/day
1.93 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 80.0 cc-mm/m²-24hr-atm
203 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
150 cc-mm/m²-24hr-atm
381 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
Melt Flow 20 g/10 min
20 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 40.0 MPa
5800 psi
ISO 527-3
Film Tensile Strength at Yield, TD 40.0 MPa
5800 psi
ISO 527-3
Film Elongation at Break, MD 600 %
600 %
ISO 527-3
Film Elongation at Break, TD 900 %
900 %
ISO 527-3
Film Elongation at Yield, MD 10 %
10 %
ISO 527-3
Film Elongation at Yield, TD 7.0 %
7.0 %
ISO 527-3
Tensile Modulus 1.10 GPa
160 ksi
conditioned; ISO 527-1/-2
3.00 GPa
435 ksi
dry; ISO 527-1/-2
Coefficient of Friction, Dynamic 0.30
0.30
ISO 8295
Tear Strength 50.0 kN/m
285 pli
Trouser Tear resistance MD; ISO 6383-1
50.0 kN/m
285 pli
Trouser Tear resistance TD; ISO 6383-1
Elmendorf Tear Strength MD 1530 g
1530 g
ISO 6383-2
Elmendorf Tear Strength TD 1530 g
1530 g
ISO 6383-2
Film Tensile Strength at Break, MD 100 MPa
14500 psi
ISO 527-3
Film Tensile Strength at Break, TD 90.0 MPa
13100 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Gloss 100 %
100 %
60°; ISO 2813
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Packaging Medical packaging
Non oriented film
Oriented film
Paper coating
Tubes
Processing Blown Film Extrusion
Film Extrusion
Other Extrusion
Product Attributes Barrier Properties
High viscosity
Nucleated