Physical Properties Metric English Comments
Carbon Dioxide Transmission 0.0240 cc-mm/m²-24hr-atm
0.0610 cc-mil/100 in²-24hr-atm
Dry; ASTM D1434
Petromont 2200 High Density Polyethylene Resin
Pétromont HDPE 2200 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This resin can be used in a mono layer or co-extrusion resin in applications requiring impr..