Polymer Property : Moisture Vapor Transmission = 47.2 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman 1810F Polyethylene  (discontinued **)
Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good opt..
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman 1830F Polyethylene  (discontinued **)
Polyethylene 1830F is a low-density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat sealing range and..
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman 1840F Polyethylene  (discontinued **)
Polyethylene 1840F is a low-density formulation with no slip or antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is characterized by..
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman E6838-795F Polyethylene  (discontinued **)
E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag..
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman E6838-796F Polyethylene  (discontinued **)
E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen..
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman E6838-922F Polyethylene  (discontinued **)
E6838-922F is a low density formulation with medium slip and medium antiblock. Outstanding optical properties make this material an excellent choice for food packaging applications.List of Applicat..
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman E6838-923F Polyethylene  (discontinued **)
E6838-923F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good clarit..
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman E6838-969F Polyethylene  (discontinued **)
E6838-969F is a low density formulation with no slip and medium antiblock. It is suggested for film applications that require toughness such as shrink/bundling film, disposable diapersand overwrap...
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman E6838-997F Polyethylene  (discontinued **)
E6838-997F natural is a low density formulation with no slip or antiblock. Outstanding optical properties make this material an excellent choice for calendering and as a clarity filler in co-extrud..
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman D4036-F Polyethylene  (discontinued **)
D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener..
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman D4052-F Polyethylene  (discontinued **)
D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance...
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman E6838-963F Polyethylene  (discontinued **)
E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..
Moisture Vapor Transmission 18.6 cc-mm/m²-24hr-atm
47.2 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman E6838-975F Polyethylene  (discontinued **)
E6838-975F is a low density formulation with medium slip and medium antiblock. The formula is used in general purpose packaging where impact strength and processability are important. End-use film..