Polymer Property : Moisture Vapor Transmission = 2.31 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.910 cc-mm/m²-24hr-atm
2.31 cc-mil/100 in²-24hr-atm
ASTM 1249
DuPont™ Clysar® LE Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film with the lowest shrink force available in the Clysar® line. Dupont Clysar® LES is ..
Moisture Vapor Transmission 0.910 cc-mm/m²-24hr-atm
2.31 cc-mil/100 in²-24hr-atm
g-mm/m²-day; based on 1 mil (0.0254 mm) thick film; ASTM E96
DuPont Elvax® 3130 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Moisture Vapor Transmission 0.910 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
2.31 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
g-mm/m²-day; based on film thickness; ASTM E96; ASTM E96
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown
12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi..