Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.910 cc-mm/m²-24hr-atm | 2.31 cc-mil/100 in²-24hr-atm | ASTM 1249 |
DuPont™ Clysar® LE Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film with the lowest shrink force available in the Clysar® line. Dupont Clysar® LES is .. |
|||
Moisture Vapor Transmission | 0.910 cc-mm/m²-24hr-atm | 2.31 cc-mil/100 in²-24hr-atm | g-mm/m²-day; based on 1 mil (0.0254 mm) thick film; ASTM E96 |
DuPont Elvax® 3130 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Moisture Vapor Transmission | 0.910 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
2.31 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
g-mm/m²-day; based on film thickness; ASTM E96; ASTM E96 |
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown 12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |