Polymer Property : Moisture Vapor Transmission = 0.889 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.230 - 0.350 cc-mm/m²-24hr-atm
0.584 - 0.889 cc-mil/100 in²-24hr-atm
Average value: 0.273 cc-mm/m²-24hr-atm Grade Count:6
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and..