Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.320 cc-mm/m²-24hr-atm
0.813 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont™ Sclairfilm® BL-1 LLDPE Film, PVDC Coated, 51 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A one-side PVDC-coated LLDPE sealant film, which provides excellent barrier properties, while retaining the outstanding physical and seal strength characte..