Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.220 cc-mm/m²-24hr-atm | 0.559 cc-mil/100 in²-24hr-atm | ASTM F1249 |
Chevron Phillips HiD® 9640 HDPE Blown Film Resin
(discontinued **) Copolymerization Enhances Film Toughness, Unique Combination of Density and Melt Index, Excellent Strength Properties as well as Good Heat Seal, Lower Density Imparts a Softer Feel and Lesser Tenden.. |
|||
Moisture Vapor Transmission | 0.220 cc-mm/m²-24hr-atm | 0.559 cc-mil/100 in²-24hr-atm | Proc. E; ASTM E96 |
DuPont Teijin Films Mylar® OB01 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB01 (formerly known as XM924) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and a polyvinylidene chlor.. |
|||
Moisture Vapor Transmission | 0.220 cc-mm/m²-24hr-atm | 0.559 cc-mil/100 in²-24hr-atm | Proc. E; ASTM E96 |
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo.. |
|||
Moisture Vapor Transmission | 0.220 cc-mm/m²-24hr-atm | 0.559 cc-mil/100 in²-24hr-atm | Proc. E; ASTM E96 |
DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the op.. |