Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 370 hour | 370 hour | F50; ASTM D1963A |
ExxonMobil HDPE HD 9830.02 High Density Polyethylene Resin Product Description: HD 9830.02 is a blow molding grade high density polyethylene copolymer with a bimodal molecular weight distribution. It provides a very good balance of stress crack resistance, .. |