Material Notes:
Product Description: HD 9830.02 is a blow molding grade high density polyethylene copolymer with a bimodal molecular weight distribution. It provides a very good balance of stress crack resistance, stiffness and impact strength with excellent processability due to its next generation branched structure.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: NoUV Stabilizer: NoApplications: Blow MoldingDrainage PipesPersonal CareSheet ExtrusionInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ASTM D4883
ESCR 100% Igepal® 370 hour
370 hour
F50; ASTM D1963A
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.8 MPa
2000 psi
ASTM D638
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790B
Tensile Impact Strength 273 kJ/m²
130 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Melting Point <= 261 °C
<= 502 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 127 °C
261 °F
ASTM D1525
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746
Users viewing this material also viewed the following: