Physical Properties Metric English Comments
ESCR 100% Igepal® >= 1500 hour
>= 1500 hour
Condition C, F<sub>50</sub>; ASTM D1693
Formosa Plastics Formolene® HL3812 Film (Hexene) HDPE
Medium Density Polyethylene Formolene® HL3812 is a high molecular weight hexene copolymer resin that is tailored specifically for geomembrane applications. The resin provides an excellent balance o..
ESCR 100% Igepal® >= 1500 hour
>= 1500 hour
Condition C; ASTM D1693
Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion
Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRBroad fusion rangeExcellent melt strengthGood processabilityExcellent flexibilityImproved output and texturingApplications: Coextruded ca..
ESCR 100% Igepal® >= 1500 hour
>= 1500 hour
Cond. C; 100% Igepal®; F<sub>50</sub>; ASTM D1693
Chevron Phillips Marlex® K307 MDPE Hexene Copolymer
Extrusion grade hexene copolymerCharacteristics: good processability, excellent melt strength, broad fusion range, outstanding stress crack resistance, meets the requirements of GRI-GM13. Meets A..
ESCR 100% Igepal® >= 1500 hour
>= 1500 hour
Cond. B; 10% Igepal®; F<sub>50</sub>; ASTM D1693
Chevron Phillips Marlex® K307 MDPE Hexene Copolymer
Extrusion grade hexene copolymerCharacteristics: good processability, excellent melt strength, broad fusion range, outstanding stress crack resistance, meets the requirements of GRI-GM13. Meets A..
ESCR 100% Igepal® >= 1500 hour

@Temperature 50.0 °C
>= 1500 hour

@Temperature 122 °F
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693
Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-7340 NT 7 LLDPE resin is well-suited for use in blow molding applications such as small, squeezable bottles, as well as, extruded flexible hoses and tubing. DOW DMDA-7340 NT 7 resin is als..
ESCR 100% Igepal® >= 1500 hour

@Temperature 50.0 °C
>= 1500 hour

@Temperature 122 °F
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693
Dow UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE)
Good extrudability/processability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6147 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This produ..
ESCR 100% Igepal® >= 1500 hour

@Temperature 50.0 °C
>= 1500 hour

@Temperature 122 °F
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693
Dow UNIVAL™ DMDC-6145 NT 7 High Density Polyethylene Resin (HDPE)
Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6145 NT 7 provides good parison stability, which contribu..