Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 97 cm³/g | 97 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® B 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Viscosity Test | 97 cm³/g | 97 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® BF 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |