Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 83 cm³/g | 83 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® B 4235 Z 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, impact modified |
|||
Viscosity Test | 83 cm³/g | 83 cm³/g | DAM; sulphuric acid 96%; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Zytel 77G33L BK031 is a 33% glass fiber reinforced black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity Test | 83 cm³/g | 83 cm³/g | DAM; sulphuric acid 96%; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL BK083 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |