Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 48 cm³/g | 48 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® G4F 23 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 48 cm³/g | 48 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 48 cm³/g | 48 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® G6F 23 R Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 48 cm³/g | 48 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 48 cm³/g | 48 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® SF 2230 Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 48 cm³/g | 48 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® G6F 23 UR Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 48 cm³/g | 48 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® SF 2220 Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 48 cm³/g | 48 cm³/g | Viscosity number |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
Viscosity Test | 48 cm³/g | 48 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® G8F 23 R Polycarbonate-40% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |