Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 470 - 4300 cm³/g | 470 - 4300 cm³/g | Average value: 2730 cm³/g Grade Count:8 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Viscosity Test | 470 cm³/g | 470 cm³/g | Intrinsic; ASTM-D4020 |
Braskem Idealis 500 Compression Molding High Molecular Weight Polyethylene Braskem Idealis 500 is the only high molecular weight polyethylene resin in powder form specially designed for the compression molding process. Its applications range from food handling, cutting boa.. |