Physical Properties Metric English Comments
Viscosity Test 280 cm³/g
280 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop..
Viscosity Test 280 cm³/g
280 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® FG42L NC010 Nylon 66  (Unverified Data**)
Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers
Viscosity Test 280 cm³/g
280 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66  (Unverified Data**)
Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Viscosity Test 280 cm³/g
280 cm³/g
Viscosity Number
DSM Akulon® S240-C Nylon 66 (European Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..