Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 175 - 220 cm³/g | 175 - 220 cm³/g | Average value: 187 cm³/g Grade Count:7 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Viscosity Test | 175 cm³/g | 175 cm³/g | Viscosity Number |
DSM Stanyl® TW300 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |