Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 168 cm³/g | 168 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Viscosity Test | 168 cm³/g | 168 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66
(Unverified Data**) 20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf.. |