Polymer Property : Viscosity Test = 146 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 146 cm³/g
146 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® AKV 30 H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding-grade, 30% glass fibers, good heat-ageing resistance
Viscosity Test 146 cm³/g
146 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules
Viscosity Test 146 cm³/g
146 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber
PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance
Viscosity Test 146 cm³/g
146 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® AKV 15 000000 Nylon 66, 15% Glass Fiber
PA 66, injection molding grade, 15% glass fibers
Viscosity Test 146 cm³/g
146 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® AKV 15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, injection molding grade, 15% glass fibers, good heat-ageing resistance