Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 112 cm³/g | 112 cm³/g | Viscosity Number |
Arkema Group Lacovyl® GB 1150 M PVC, Pipe Grade LACOVYL GB 1150 M is a vinyl chloride homopolymer produced by the Elf Atochem's mass polymerization process.Its characteristics are : Viscosity index (ISO 1628-2):112 ml/g,(K value:67). Apparen.. |
|||
Viscosity Test | 112 cm³/g | 112 cm³/g | Viscosity Number |
Arkema Group Lacovyl® S 110 P PVC LACOVYL S 110 P is a vinyl chloride homopolymer produced by a suspension polymerization process.Characteristics : Viscosity index (ISO 1628-2):112 ml/g,(K value:67). Apparent density (ISO 60):0.56 g.. |
|||
Viscosity Test | 112 cm³/g | 112 cm³/g | Viscosity number |
BASF Ultradur B 4406 G4 Q113 20% Glass Filled PBT Ultradur B4406 G4 Q113 is an UL V0 injection molding PBT grade with 20% glass fiber reinforcement. |