Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 1.70 - 3.20 mm | 0.0669 - 0.126 in | |
Ineos Nova T163B Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for very low density foam.Applications: This grade is used mainl.. |