Material Notes:
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for very low density foam.Applications: This grade is used mainly for producing very low density block. A typical application is drainage boards.Information provided by NOVA Chemicals.
Physical Properties Metric English Comments
Bulk Density 0.620 g/cc
0.0224 lb/in³
Density 0.00900 - 0.0150 g/cc
0.000325 - 0.000542 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
>= 0.0120 g/cc
>= 0.000434 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
Bead Size 1.70 - 3.15 mm
0.0669 - 0.124 in
> 95% in this range per Berre Laboratory Analytical Methods 0492
1.70 - 3.20 mm
0.0669 - 0.126 in
Chemical Properties Metric English Comments
Blowing Agent Content >= 5.9 %
>= 5.9 %