Physical Properties Metric English Comments
Bead Size 1.25 - 2.50 mm
0.0492 - 0.0984 in
IRPC Polimaxx Pentfoam 193L Expandable Polystyrene
General: Pentfoam 139L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application..
Bead Size 1.25 - 2.50 mm
0.0492 - 0.0984 in
IRPC Polimaxx Pentfoam 241F Expandable Polystyrene
General: Pentfoam 241F is a regular grade expandable polystyrene containing pentane as blowing agentApplications: Pentfoam 241F is particularly well suited for the manufacture of eps insulation boar..