IRPC Polimaxx Pentfoam 241F Expandable Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer IRPC Polimaxx
Trade Name Pentfoam
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Pentfoam 241F Expandable Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General: Pentfoam 241F is a regular grade expandable polystyrene containing pentane as blowing agentApplications: Pentfoam 241F is particularly well suited for the manufacture of eps insulation boards, block. This grade is also widely used for the production of low density decoration products, and road construction block.
Physical Properties Metric English Comments
Density 0.0120 - 0.0130 g/cc
0.000434 - 0.000470 lb/in³
0.0120 - 0.0200 g/cc
0.000434 - 0.000723 lb/in³
molding density range
Bead Size 1.25 - 2.50 mm
0.0492 - 0.0984 in
Maximum Moisture Content 0.20
0.20
Mechanical Properties Metric English Comments
K Factor (Wear Factor) 56 - 58
56 - 58
Chemical Properties Metric English Comments
Blowing Agent Content >= 6.0 %
>= 6.0 %