Polymer Property : Bead Size = 0.0197 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bead Size 0.300 - 0.500 mm
0.0118 - 0.0197 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Styrocell® D833A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic..
Bead Size 0.350 - 0.500 mm
0.0138 - 0.0197 in
NOVA Chemicals Styrocell® D833A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic..
Bead Size 0.300 - 0.500 mm
0.0118 - 0.0197 in
Iran Petrochemical (PCC) TPC - 522 FC Expandable Polystyrene
TPC - 522 FCApplications: shape molding with wall thickness
Bead Size 0.300 - 0.500 mm
0.0118 - 0.0197 in
Iran Petrochemical (PCC) TPC - 526 WP Expandable Polystyrene
TPC - 526 WPApplications: very thin-wall water proof shape molding products with wall thickness
Bead Size 0.350 - 0.500 mm
0.0138 - 0.0197 in
JIS Z8801
Samsung Cheil Industries Starex® SG-501 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.
Bead Size 0.350 - 0.500 mm
0.0138 - 0.0197 in
JIS Z8801
Samsung Cheil Industries Starex® SG-501 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.