Polymer Property : High Load Melt Index = 7.8 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
High Load Melt Index 7.8 g/10 min

@Load 21.6 kg,
Temperature 200 °C
7.8 g/10 min

@Load 47.6 lb,
Temperature 392 °F
Ashley Polymers Ashlene® PC/ABS Alloy
Flame retardant alloy.Data provided by the manufacturer