Ashley Polymers Ashlene® PC/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® PC/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant alloy.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
High Load Melt Index 7.8 g/10 min

@Load 21.6 kg,
Temperature 200 °C
7.8 g/10 min

@Load 47.6 lb,
Temperature 392 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ATSM D638
Elongation at Break 52 %
52 %
ASTM D638
Flexural Strength 79.0 MPa
11500 psi
ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 4.33 J/cm
8.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in