Polymer Property : High Load Melt Index = 50 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
High Load Melt Index 50 g/10 min

@Load 21.6 kg
50 g/10 min

@Load 47.6 lb
ISO 1133
Total Finathene® 6006 HDPE, blow molding, pipe  (discontinued **)
Finathene® 6006 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Polymerization is conducted in the absence of any other comonomer. Finathene® 6006 h..
High Load Melt Index 50 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Meilian Chemical PE2280 BLACK MASTERBATCH
BLACK PE2280 is an economy , high tinting strength black masterbatch based on LDPE containing high opacity carbon black. It is designed for use in jet black, high gloss injection molding items, shee..
High Load Melt Index 50 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Meilian Chemical PE-B1301 BLACK MASTERBATCH
BLACK PE-B1301 is a black low density polyethylene based masterbatch containing pure high opacity carbon black. It is designed for use in high jet black film with excellent surface performance, such..
High Load Melt Index 50 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Meilian Chemical PE401A GREEN MASTERBATCH
GREEN PE 401A is a green LDPE based masterbatch containing 16% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Green 7.Method of Usage: GREEN PE 401A is designed f..