Meilian Chemical PE401A GREEN MASTERBATCH

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Meilian Chemical Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Meilian Chemical PE401A GREEN MASTERBATCH.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GREEN PE 401A is a green LDPE based masterbatch containing 16% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Green 7.Method of Usage: GREEN PE 401A is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, avoiding pollution and malscattering problems caused by pigmentRange of Application: GREEN PE 401A is designed for use in LDPE, HDPE, LLDPE and PP for production of premium high gloss films with optimum printability.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
High Load Melt Index 50 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Descriptive Properties Value Comments
Carrier LDPE
Compatibility LDPE, HDPE, PP and Ethylene copolymer
Pigment Content 16