Polymer Property : High Load Melt Index = 130 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
High Load Melt Index 130 g/10 min

@Load 21.6 kg,
Temperature 250 °C
130 g/10 min

@Load 47.6 lb,
Temperature 482 °F
BASF Luranyl® KR 2450/3 Polyphenylene Ether + Styrene-Butadiene Blend
Easy-flowing grade containing halogen-free, flame-retardant. Uses include: housings for electrical appliances, tubular wiring conduits, tachograph housings.Data was collected by ISO methods and pro..
High Load Melt Index 130 g/10 min

@Load 21.5 kg,
Temperature 250 °C
130 g/10 min

@Load 47.4 lb,
Temperature 482 °F
BASF Luranyl® KR 2451/3 Polyphenylene Ether + Styrene-Butadiene Blend
Especially easy flowing grade containing halogen-free, flame-retardant; mainly used for housings for electrical equipment and in the electronics sector.Data was collected by ISO methods and provided..