Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 0.10 g/10 min @Load 21.6 kg, Temperature 190 °C |
0.10 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
LyondellBasell Lupolen® 4261 A HDPE, Blow Molding Grade Easy-to-process bow molding grade for technical containers such as fuel tanks, petrol filler inlets, expansion tanks, horticultural spray tanks, tanks for lawnmowers, disposable containers (up to 10.. |
|||
High Load Melt Index | 0.10 g/10 min @Load 21.6 kg, Temperature 190 °C |
0.10 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
LyondellBasell Lupolen® 5261 Z HDPE, Blow Molding Grade Relatively high viscosity blow molding grade for rigid, stackable and highly shock resistant containers for packaging all types of hazardous materials such as flammable, corrosive, poisonous and sur.. |
|||
High Load Melt Index | 0.10 g/10 min @Load 21.6 kg, Temperature 190 °C |
0.10 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
LyondellBasell Lupolen® 5261 Z HI HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
High Load Melt Index | 0.10 g/10 min @Load 21.6 kg, Temperature 190 °C |
0.10 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of.. |