Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 36.3 dynes/cm | 36.3 dynes/cm | Harmonic Mean - Dispersive |
Eastman Embrace HY1000 Copolyester for Shrink Film Applications:Beverage packagingCosmetics/personal care packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingKey Attributes:Eye catching 360° graphic capabilityNoise-free shr.. |
|||
Surface Tension | 36.3 dynes/cm | 36.3 dynes/cm | Harmonic Mean - Total |
Eastman Embrace HY1000 Copolyester for Shrink Film Applications:Beverage packagingCosmetics/personal care packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingKey Attributes:Eye catching 360° graphic capabilityNoise-free shr.. |