Physical Properties Metric English Comments
Surface Tension 17.4 dynes/cm
17.4 dynes/cm
Dow Corning XIAMETER® PMCPPMX-200 1CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 1CS. A polydimethylsiloxane polymer for use in skincare, suncare, woundcare, hair care, and color cosmetic applications. INCI Name: TrisiloxaneInf..
Surface Tension 17.4 dynes/cm
17.4 dynes/cm
Dow Corning 200® 1 CST FLUID
A polydimethylsiloxane polymer for use in skincare, suncare, woundcare, hair care, and color cosmetic applications.Information provided by Dow Corning