Dow Corning XIAMETER® PMCPPMX-200 1CS Silicone Fluid

Category Fluid
Manufacturer Dow Corning
Trade Name XIAMETER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning XIAMETER® PMCPPMX-200 1CS Silicone Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is chemically equivalent to DOW CORNING® 200 FLUID 1CS. A polydimethylsiloxane polymer for use in skincare, suncare, woundcare, hair care, and color cosmetic applications. INCI Name: TrisiloxaneInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.820 g/cc

@Temperature 25.0 °C
0.820 g/cc

@Temperature 77.0 °F
Viscosity Measure 1.0 cSt
1.0 cSt
Kinetic/Kinematic
Surface Tension 17.4 dynes/cm
17.4 dynes/cm
Thermal Properties Metric English Comments
Flash Point >= 30.0 °C
>= 86.0 °F
Closed Cup
Optical Properties Metric English Comments
Refractive Index 1.38
1.38
Descriptive Properties Value Comments
Cyclotetrasiloxane Content (max %) 0.5