Surface Tension 16.9 dynes/cm
16.9 dynes/cm
25°C
Asahi Glass ASAHIKLIN AK-225G Hydrochlorofluorocarbon Solvent
AK-225G is an environmentally sensible HCFC. It is thermally stable, nonflammable and recoverable by distillation with no decomposition. It has substantially lower global warming potential (GWP) th..