Asahi Glass ASAHIKLIN AK-225G Hydrochlorofluorocarbon Solvent

Category Fluid , Solvent
Manufacturer Asahi Glass Company
Trade Name ASAHIKLIN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass ASAHIKLIN AK-225G Hydrochlorofluorocarbon Solvent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AK-225G is an environmentally sensible HCFC. It is thermally stable, nonflammable and recoverable by distillation with no decomposition. It has substantially lower global warming potential (GWP) than PFCs and HFCs and an extremely low ozone depletion potential (ODP). AK-225 is exempt from VOC regulations by the U.S. EPA as described in the Oct. 8, 1996 Federal Register.Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Density 1.56 g/cc

@Temperature 25.0 °C
0.0564 lb/in³

@Temperature 77.0 °F
Liquid
Solubility of Water 0.027 %
0.027 %
25°C
Solubility in Water 0.016 %
0.016 %
25°C
Viscosity 0.60 cP

@Temperature 25.0 °C
0.60 cP

@Temperature 77.0 °F
Molecular Weight 202.94 g/mol
202.94 g/mol
Vapor Pressure 0.353 bar

@Temperature 25.0 °C
265 torr

@Temperature 77.0 °F
Surface Tension 16.9 dynes/cm
16.9 dynes/cm
25°C
Thermal Properties Metric English Comments
Heat of Vaporization 146 J/g
63.0 BTU/lb
b.p.
Specific Heat Capacity 1.088 J/g-°C

@Temperature 25.0 °C
0.2600 BTU/lb-°F

@Temperature 77.0 °F
Liquid
Melting Point -116 °C
-177 °F
Boiling Point 56.1 °C
133 °F
Descriptive Properties Value Comments
Global Warming Potential (CO2=1, 100yr ITH) 530
KB Value 30
Ozone Depletion Potential (CFC-11 = 1.0) 0.8