Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 1.5 dynes/cm | 1.5 dynes/cm | 0.5%, Light Phase: Cyclohexane |
3M Novec™ FC-4430 Fluorosurfactant 3M™ Novec™ Fluorosurfactant FC-4430 is a non-ionic polymeric fluorochemical surfactant belonging to a class of coating additives which provide low surface tensions in coating systems best served b.. |