Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Novec™ FC-4430 Fluorosurfactant

Category Fluid , Polymer , Thermoplastic , Fluoropolymer
Manufacturer 3M
Trade Name Novec™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Novec™ FC-4430 Fluorosurfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Novec™ Fluorosurfactant FC-4430 is a non-ionic polymeric fluorochemical surfactant belonging to a class of coating additives which provide low surface tensions in coating systems best served by fluorochemical surfactants. Novec fluorosurfactant FC-4430 contributes excellent wetting, spreading and leveling properties to a variety of coating systems.Information provided by 3M
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
pH 4.5
4.5
1% aqueous solution
Viscosity 2000 - 6000 cP
2000 - 6000 cP
Vapor Pressure 0.0000930 bar
0.0698 torr
Surface Tension 1.5 dynes/cm
1.5 dynes/cm
0.5%, Light Phase: Cyclohexane
2.2 dynes/cm
2.2 dynes/cm
0.5%, Light Phase: Heptane
2.5 dynes/cm
2.5 dynes/cm
200 ppm, Light Phase: Cyclohexane
3.2 dynes/cm
3.2 dynes/cm
200 ppm, Light Phase: Heptane
Thermal Properties Metric English Comments
Glass Transition Temp, Tg <= 0.000 °C
<= 32.0 °F
Flash Point 82.0 °C
180 °F
Setaflash closed cup