Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 60 - 80 Mesh | 60 - 80 Mesh | US Sieve |
Potters Industries A-Series P-0100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Mesh Size | 60 - 100 Mesh | 60 - 100 Mesh | |
Potters Industries Spheriglass® 1922 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 5% max retained; SABIC (PVC 003) |
SABIC PVC 59S Suspension Polyvinyl Chloride for Rigid Products Product Description: PVC 59S is a free flowing vinyl chloride homopolymer resin having low molecular weight. It is manufactured by suspension polymerization.Characteristics: PVC 59S has the follo.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 15% max retained; SABIC (PVC 003) |
SABIC PVC 67S Suspension Polyvinyl Chloride for Rigid Extruded Products Product Description: PVC 67S is a free flowing vinyl chloride homopolymer resin having medium molecular weight. It is manufactured by suspension polymerization.Characteristics: PVC 67S has the fo.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 15% max retained; SABIC (PVC 003) |
SABIC PVC 70S Suspension Polyvinyl Chloride for Flexible Products Product Description: PVC 70S is a free flowing vinyl chloride homopolymer resin having a high molecular weight. It is manufactured by suspension polymerization.Characteristics: PVC 70S has the fo.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 5% Retention; PVCH/QCD/3514 |
Reliance Industries 57-01 Polyvinyl Chloride Information provided by Reliance IndustriesApplications: Rigid injection. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 5% Retention; PVCH/QCD/3514 |
Reliance Industries 60-11 Polyvinyl Chloride Information provided by Reliance IndustriesApplications:Recommended:Rigid extrusionRigid injectionRigid calenderingCan be used:Blow molding |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 10% Retention; PVCH/QCD/3514 |
Reliance Industries 67-11 Polyvinyl Chloride Information provided by Reliance IndustriesApplications: Recommended:Flexible extrusionFlexible injectionFlexible calenderingCan be used:Rigid injectionRigid extrusion |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 5% Retention; PVCH/QCD/3514 |
Reliance Industries 57-11 Polyvinyl Chloride Information provided by Reliance IndustriesApplications: Rigid injectionRigid extrusionRigid calenderingblow molding |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
Chevron Phillips Ryton® PR37 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 75 wt% Passing |
Chevron Phillips Ryton® PR26 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
Chevron Phillips Ryton® PR25 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 75 wt% Passing |
Chevron Phillips Ryton® PR27 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 75 wt% Passing |
Chevron Phillips Ryton® PR34 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 75 wt% Passing |
Chevron Phillips Ryton® PR35 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
Chevron Phillips Ryton® PR06 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 75 wt% Passing |
Chevron Phillips Ryton® PR39 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
Chevron Phillips Ryton® P-4 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
Solvay Specialty Polymers Ryton® P-6 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 0.05% retained |
Imerys Kaolexâ„¢ FG Kaolin Kaolex FG is a air floated Hydrated Aluminum Silicate. Its low surface area makes it a good choice for fiberglass manufacturing.Information provided by Imerys |
|||
Particle Mesh Size | 60 - 100 Mesh | 60 - 100 Mesh | 0.0021 |
Gromax Melamine (Fine Grade) China KInformation provided by Gromax Enterprises Corp. |
|||
Particle Mesh Size | 60 - 100 Mesh | 60 - 100 Mesh | 0.1623 |
Gromax Standard GB9567-97 China NInformation provided by Gromax Enterprises Corp. |
|||
Particle Mesh Size | 60 - 100 Mesh | 60 - 100 Mesh | 0.1973 |
Gromax Standard GB9567-97 China SInformation provided by Gromax Enterprises Corp. |
|||
Particle Mesh Size | >= 60 Mesh | >= 60 Mesh | 80%; ASTM E11-87 |
Minelco FireCarb TEG-160 Expandable Graphite High quality crystalline flake graphite that has a medium to high source of carbon, typically 80 – 99%Expandable graphite belongs to a group of products called "intumescents." The primary prope.. |
|||
Particle Mesh Size | 60 - 80 Mesh | 60 - 80 Mesh | |
Beijing Evergrow Resources ACFP-60 Activated Carbon Fiber Powder Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral contentApplicatio.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 10% Retention; PVCH/QCD/3514 |
Reliance Industries 70-21 Polyvinyl Chloride Information provided by Reliance IndustriesApplications:Can be used:Flexible extrusionFlexible injectionFlexible calendering |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
Chevron Phillips Ryton® PR33 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 95 wt% Passing |
Solvay Specialty Polymers Ryton® PR11 Polyphenylene Sulfide Resin
(Unverified Data**) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 99.5 wt% Passing |
Solvay Specialty Polymers Ryton® V-1 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantApplications: CoatingsInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |
|||
Particle Mesh Size | 60 Mesh | 60 Mesh | 95 wt% Passing |
Chevron Phillips Ryton® PR11 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |