SABIC PVC 67S Suspension Polyvinyl Chloride for Rigid Extruded Products

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer SABIC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC PVC 67S Suspension Polyvinyl Chloride for Rigid Extruded Products.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: PVC 67S is a free flowing vinyl chloride homopolymer resin having medium molecular weight. It is manufactured by suspension polymerization.Characteristics: PVC 67S has the following properties that make it suitable for rigid PVC processing with high production rates: Easy handling and conveyingVery low dust levelHigh purityHigh bulk densityNarrow particle size distributionPVC 67S is designed to give an easy processing product for rigid applications since it has a low melt viscosity. It can be used with a wide range of heat stabilizers.Typical Applications: ExtrusionRigid pipes (pressure and non-pressure)Rigid profilesCorrugated tubes and conduitsInformation provided by SABIC.
Physical Properties Metric English Comments
Volatiles <= 0.30 %
<= 0.30 %
ASTM D3030
Apparent Bulk Density 0.570 g/cc
0.0206 lb/in³
ASTM D1895
Particle Mesh Size 60 Mesh
60 Mesh
15% max retained; SABIC (PVC 003)
200 Mesh
200 Mesh
4% max passing through; SABIC (PVC 003)
Descriptive Properties Value Comments
K-Value 67
DIN 53726