Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 14 Mesh | 14 Mesh | Opening 1700µm; ASTM E11 |
Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS Some applications of this product may be regulated or restricted by national or international standards (e.g. for food additives, water treatment, the pharmaceutical industry, etc). The buyer and th.. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® 2751-00 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi.. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® 461 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® 2821-00 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi.. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® 301-F Polyvinylidene Fluoride Powder Characteristics: Fine milled, white, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abra.. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® 711 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® 721 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® 741 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® LBG1 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® LBG2 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® HSV Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® 201 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® 2501-20 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Very flexible, very soluble. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low p.. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® 2801-00 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi.. |
|||
Particle Mesh Size | 14 Mesh | 14 Mesh | |
Arkema Group KYNAR® 761 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |
|||
Particle Mesh Size | 14 - 18 Mesh | 14 - 18 Mesh | US Sieve |
Potters Industries A-Series A-120 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |