Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 35000 - 90000 cP | 35000 - 90000 cP | RVF #6 sp @ 20 rpm |
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsHigh viscosity grade adhesive for many brush or spray applications.Quick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Brookfield Viscosity | 45000 - 90000 cP | 45000 - 90000 cP | Base, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ DP100 FR Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 FR is a two-part flame retardant (self-extinguishing) version of Scotch-Weld DP100. It meets the UL94 V-O Burn Test requirements and has a work life of 4-8 mi.. |
|||
Brookfield Viscosity | 50000 - 90000 cP | 50000 - 90000 cP | RVT 'T-spindle' C @ 2.5 |
3M Scotch-Weld™ PR Gel Plastic and Rubber Instant Adhesive 3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates .. |
|||
Brookfield Viscosity | 50000 - 90000 cP | 50000 - 90000 cP | RVT 'T-spindle' C @ 2.5 rpm |
3M Scotch-Weld™ SI Gel Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI Gel (formerly SB09) is a fas.. |