Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Strong flexible bondsHigh viscosity grade adhesive for many brush or spray applications.Quick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, gasketing materials to a variety of substratesMay be heat cured to obtain improved physical properties.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 46 - 55 %
46 - 55 %
Brookfield Viscosity 35000 - 90000 cP
35000 - 90000 cP
RVF #6 sp @ 20 rpm
Mechanical Properties Metric English Comments
Shear Strength 0.0621 MPa

@Temperature 82.0 °C
9.00 psi

@Temperature 180 °F
Overlap, 1/8" Birch/Birch
0.138 MPa

@Temperature 66.0 °C
20.0 psi

@Temperature 151 °F
Overlap, 1/8" Birch/Birch
1.05 MPa

@Temperature 1.00 °C
152 psi

@Temperature 33.8 °F
Overlap, 1/8" Birch/Birch
1.38 MPa

@Temperature 14.0 °C
200 psi

@Temperature 57.2 °F
Overlap, 1/8" Birch/Birch
Peel Strength 0.701 kN/m

@Temperature 14.0 °C,
Time 1.81e+6 sec
4.00 pli

@Temperature 57.2 °F,
Time 504 hour
180°, Canvas/Steel
1.58 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
9.00 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
2.28 kN/m

@Temperature 14.0 °C,
Time 86400 sec
13.0 pli

@Temperature 57.2 °F,
Time 24.0 hour
180°, Canvas/Steel
2.80 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
16.0 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
3.51 kN/m

@Temperature 1.00 °C,
Time 1.81e+6 sec
20.0 pli

@Temperature 33.8 °F,
Time 504 hour
180°, Canvas/Steel
4.12 kN/m

@Temperature 14.0 °C,
Time 259000 sec
23.5 pli

@Temperature 57.2 °F,
Time 72.0 hour
180°, Canvas/Steel
4.82 kN/m

@Temperature 14.0 °C,
Time 432000 sec
27.5 pli

@Temperature 57.2 °F,
Time 120 hour
180°, Canvas/Steel
5.43 kN/m

@Temperature 14.0 °C,
Time 605000 sec
31.0 pli

@Temperature 57.2 °F,
Time 168 hour
180°, Canvas/Steel
6.14 kN/m

@Temperature 14.0 °C,
Time 1.21e+6 sec
35.0 pli

@Temperature 57.2 °F,
Time 336 hour
180°, Canvas/Steel
Thermal Properties Metric English Comments
Flash Point -18.0 °C
-0.400 °F
CC
Descriptive Properties Value Comments
Appearance Dark Brown
Base Nitrile Rubber