Physical Properties Metric English Comments
Brookfield Viscosity 750000 - 1.10e+6 cP
750000 - 1.10e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-360 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-360 Class B are fast cure, intermediate density two-component, manganese dioxide cure, polysulfide fuel tank and fuselage sealant. 3M AC-360 Class B Sealants have outstanding..
Brookfield Viscosity 750000 - 1.10e+6 cP
750000 - 1.10e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-360 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-360 Class B are fast cure, intermediate density two-component, manganese dioxide cure, polysulfide fuel tank and fuselage sealant. 3M AC-360 Class B Sealants have outstanding..