Material Notes:
3M Aerospace Sealant AC-360 Class B are fast cure, intermediate density two-component, manganese dioxide cure, polysulfide fuel tank and fuselage sealant. 3M AC-360 Class B Sealants have outstanding resistance to aviation gasoline and jet fuel, as well as resistance to chemicals and petroleum products common to the aircraft industry. 3M AC-360 Class B Sealants maintain flexibility and bond strength on most metal substrates such as aluminum, titanium, steel, stainless steel, and many coatings under extremes of temperature, weathering and stress. The mixed compound is a thixotropic paste easily applied by extrusion, injection gun or spatula. It has excellent tooling properties.Information provided by 3M
Physical Properties Metric English Comments
Density <= 1.40 g/cc
<= 0.0506 lb/in³
cured 14 days @ 50% RH
Volatiles 2.0 %
2.0 %
Brookfield Viscosity 750000 - 1.10e+6 cP
750000 - 1.10e+6 cP
Base, RVF #7 sp @ 2 rpm
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 55
50 - 55
cured 14 days @ 50% RH
Tensile Strength at Break 1.10 MPa
160 psi
7 days in BMS-3-11 ty IV
1.90 MPa
276 psi
Standard Cure
2.07 MPa
300 psi
7 days JRF
Elongation at Break 550 %
550 %
Standard Cure
780 %
780 %
7 days JRF
800 %
800 %
7 days in BMS-3-11 ty IV
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
cured 14 days @ 50% RH
182 °C
360 °F
Short term, cured 14 days @ 50% RH
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
cured 14 days @ 50% RH
Processing Properties Metric English Comments
Cure Time 120 - 180 min
2.00 - 3.00 hour
Tack-Free Time
120 - 180 min
2.00 - 3.00 hour
Shelf Life 6.00 Month

@Temperature <=26.7 °C
6.00 Month

@Temperature <=80.1 °F
Descriptive Properties Value Comments
Appearance Brown