Polymer Property : Brookfield Viscosity = 7000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 5000 - 7000 cP

@Temperature 25.0 °C
5000 - 7000 cP

@Temperature 77.0 °F
HBT, Spindle CP-51 @ 10rpm
Lord Adhesives 6144 Silver Conductor
LORD 6144 silver conductor is a one-component, thermosetting conductive epoxy designed for surface mount attachment of electronic component devices. It is primarily used as a chip-to-lead frame adhe..