Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 5000 - 9000 cP | 5000 - 9000 cP | DOP 60phr, 6RPM; ASTM D1824-90 |
LG Chemical LK170 PVC General Description: LK170, vinyl chloride copolymer with vinyl acetate exhibit excellent properties including easy processing and effective flowMain Applications: Sealant, automotive protective sol.. |
|||
Brookfield Viscosity | 5000 - 7000 cP @Temperature 25.0 °C |
5000 - 7000 cP @Temperature 77.0 °F |
HBT, Spindle CP-51 @ 10rpm |
Lord Adhesives 6144 Silver Conductor LORD 6144 silver conductor is a one-component, thermosetting conductive epoxy designed for surface mount attachment of electronic component devices. It is primarily used as a chip-to-lead frame adhe.. |
|||
Brookfield Viscosity | <= 5000 cP | <= 5000 cP | Spindle # 4, rpm 60 |
Michelman® Michem® Glide 37 Nonionic PTFE dispersion Description: Nonionic PTFE dispersionUsage: Michem® Glide 37 as an additive provides mar, abrasion and high temperature resistance for a variety of applications within the paint and coating indus.. |
|||
Brookfield Viscosity | 5000 cP @Temperature 25.0 °C |
5000 cP @Temperature 77.0 °F |
25% Toluene solution; BAM 922 |
Kraton® FG1901 G (SEBS) Linear Block Copolymer Description: Kraton FG1901 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form id.. |
|||
Brookfield Viscosity | 5000 cP @Temperature 25.0 °C |
5000 cP @Temperature 77.0 °F |
|
Loctite® 3106 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 5000 cP @Temperature 25.0 °C |
5000 cP @Temperature 77.0 °F |
|
Loctite® 3321 Light Cure Acrylic Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Brookfield Viscosity | 5000 cP @Temperature 25.0 °C |
5000 cP @Temperature 77.0 °F |
|
Loctite® 3381 Light Cure Acrylic Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Brookfield Viscosity | 5000 cP | 5000 cP | 25% toluene solution; MA 04-3-064 |
Dynasol Calprene® 501 Thermoplastic Rubber SBS Dry Calprene 501 is a 69/31 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and having a linear structure.This product is available in:C 501 porous crumbC 501C porous pelletC 501M pow.. |
|||
Brookfield Viscosity | 5000 cP @Temperature 191 °C |
5000 cP @Temperature 375 °F |
|
3M Scotch-Weld™ 3792 Hot Melt Adhesive Clear, multi-purpose for wood, corrugated, fabric, fur nature, upholstery, novelties, and other lightweight materialsInformation provided by 3M |
|||
Brookfield Viscosity | 5000 - 9000 cP | 5000 - 9000 cP | Accelerator, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Brookfield Viscosity | 5000 - 6000 cP | 5000 - 6000 cP | Base, RVF #6 sp @ 20 rpm |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Brookfield Viscosity | 5000 cP @Temperature 191 °C |
5000 cP @Temperature 375 °F |
|
3M Scotch-Weld™ 3748 Hot Melt Adhesive Good thermal shock resistance; Non-corrosive to copper for many electronic applications and Bonds polyolefinesInformation provided by 3M |
|||
Brookfield Viscosity | 5000 - 10000 cP | 5000 - 10000 cP | RVT #4 spindle @ 20 rpm |
3M Scotch-Weld™ RT20 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
Brookfield Viscosity | 5000 - 10000 cP | 5000 - 10000 cP | RVT #3 sp @ 2.5 rpm |
3M Scotch-Weld™ RT3500B Rubber-Toughened Instant Adhesive 3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon.. |